Tin / Base Fine Pewter (Lead Free) A-C - Casting Alloy (Pewter)– Popular! An excellent casting pewter that contains approx 90% Tin, 8% Antimony and 2% Copper. The copper makes the metal more ductile so that it can be formed easier with a hammer if necessary. Melt Temp Around 466 deg F R-92 - Casting Alloy (Pewter)-Popular! An excellent casting alloy with approximately 92% Tin and 8% Antimony and containing no copper. Melt Temp Around 466 deg F
RotoNickel - Babbitt (Pewter) – A durable Babbitt metal consisting of approximately 89% Tin with 3.45%Copper, 7.5% Antimony and .15% of Monel which contains Nickel. Sometimes called High-Speed Nickel Babbitt or 4 X Nickel Babbitt, this Babbitt is suitable for bearings which are exposed to high temperatures and friction. Melt Temp Around 466 deg F
Lead / Base Pewter and Babbitt ( Not for use around food, or frequent human contact ) Copper- Hard Babbitt- A medium speed Babbitt metal consisting of approximately 36% Tin with 51% Lead, 1% Copper and 12% Antimony. Melt Temp Around 360 deg F Formula “0” Babbitt- A low speed Babbitt consisting of approximately 10% Tin, 75% Lead, and 15% Antimony. Melt Temp Around 464 deg F #4 Hardware Babbitt- A low speed Babbitt consisting of approximately 87.5% Lead and 12.66% Antimony. Melt Temp Around 473 deg F
Custom Pewter Alloys-Please call For a Quote!
Custom alloys, made to your specs, are available in
various quantities. Just let us know what percentages you would like and we can
alloy into ingot form for you! |